设为首页加入收藏

基于室内加速模拟的聚醚型聚氨酯铺装材料耐久性评价

作者:王安杰,杨申鹏,王士辉,谭继兴,马年先,周树宝  发布时间:2026-08-29   编辑:赵玉真   审核人:郎伟锋    浏览次数:

基于室内加速模拟的聚醚型聚氨酯铺装材料耐久性评价

王安杰,杨申鹏*,王士辉,谭继兴,马年先,周树宝

山东金曰交通发展集团有限公司,山东 济南  250101

摘要:为评估新型聚醚型聚氨酯混凝土(Polyether Polyurethane concrete,PPC)的耐久性,基于道路铺装层典型服役环境特征,采用考虑环境因素的60 ℃老化、90 ℃老化和紫外线老化3种加速老化模拟方法,通过浸水飞散、低温弯曲、车辙、冻融劈裂及四点弯曲疲劳等试验,综合表征老化后材料的抗松散性、低温抗裂性、抗永久变形能力、水稳定性及疲劳性能,并与同等级配苯乙烯-丁二烯-苯乙烯嵌段共聚物(Styrene-Butadiene-Styrene,SBS)改性沥青混合料(SBS modified asphalt mixture,SMAM)进行对比。结果表明:PPC试件在3种老化条件下的飞散强度损失率为11.07%~19.15%,均小于未老化的SMAM试件(20%);紫外线老化与热耦合老化导致PPC试件低温性能显著衰减,但PPC试件老化6周后的最大弯拉应变仍大于未老化的SMAM试件;PPC试件的动稳定度随老化时间延长而增大,老化6周后为SMAM试件的6倍以上;在各老化条件下,SMAM试件的强度衰减速率均高于PPC试件,经5次冻融循环后,PPC试件的劈裂强度为1.35 MPa,是SMAM试件的1.7倍;PPC试件在各老化条件下的疲劳寿命均超过100万次,初始弯曲劲度模量远低于SMAM试件,随冻融循环次数和老化时间的增加,SMAM试件的初始劲度模量增大,PPC试件的初始劲度模量减小。证明PPC的耐久性能显著优于传统沥青基材料。

关键词:PPC;路面铺装;路用性能;耐久性;模拟评价

Durability evaluation of Polyether Polyurethane paving materials based on indoor accelerated simulation

WANG Anjie, YANG Shenpeng*, WANG Shihui, TAN Jixing,

MA Nianxian, ZHOU Shubao

Shandong Kingyue Transportation Development Group Co., Ltd., Jinan 250101, China

Abstract: To evaluate the long-term durability of a novel Polyether Polyurethane concrete (PPC) under typical pavement service conditions, three accelerated aging simulations are conducted: 60 ℃ and 90 ℃ thermal-oxidative aging, and ultraviolet aging. The material′s post-aging resistance to raveling, low-temperature cracking, permanent deformation, water stability, and fatigue are comprehensively characterized using immersed raveling tests, low-temperature bending tests, rutting tests, freeze-thaw splitting tests, and four-point bending fatigue tests. These are compared against a control Styrene-Butadiene-Styrene modified asphalt mixture (SMAM) with an identical gradation. Results indicate that the Cantabro strength loss rates of PPC test specimen under the three aging conditions range from 11.07% to 19.15%, all lower than that of the unaged SMAM test specimen(20.00%). Although coupled UV-thermal aging degraded its low-temperature performance, the maximum flexural tensile strain of the 6 weeks aged PPC test specimen remains higher than that of the unaged SMAM test specimen. The dynamic stability of PPC test specimen increases with aging time, reaching over six times that of the SMAM test specimen after 6 weeks of aging. The strength decay rate of SMAM test specimen is higher than that of PPC test specimen under all aging conditions. Following 6 freeze-thaw cycles, the residual splitting strength of PPC test specimen(1.35 MPa) is 1.7 times that of the SMAM test specimen. Furthermore, the fatigue life of PPC test specimen exceeds 1 million cycles under all aging conditions, with an initial flexural stiffness modulus significantly lower than that of the SMAM test specimen. As the number of freeze-thaw cycles and aging time increase, the initial stiffness modulus of SMAM test specimen increases, whereas that of PPC test specimen decreases. In conclusion, the long-term durability of PPC is substantially superior to that of traditional asphalt-based materials.

Keywords: PPC; pavement paving; road performance; durability; simulation evaluation

  • 附件【XB-2026-03-13.pdf】已下载次

通信地址:济南市长清大学科技园海棠路5001号 邮编:250357
《山东交通学院学报》编辑部电话:0531-80687340
《内燃机与动力装置》编辑部电话:0531-80687025
山东交通学院学报编辑部版权所有 网站浏览次数: 次